Fused Mullite Main Parameter
Properties | elct.melt.3Al2O3.2SiO2 | |
Chemical | Al2O3 | 70-77 |
SiO2 | 22-29 | |
Fe2O3 | <0.10 | |
R2O | <0.5 | |
RO | <0.3 | |
Refractoriness (℃) | >1850 | |
Particle Bulk Density(g/cm3) | >3.03 | |
Linear Expansion Coefficient | -6.0Χ10-6 /℃ | |
Glass phase Content (%) | ≤5-6 % | |
3Al2O3.2SiO2 Phase | ≥94-95 % |
Spinel and Al2O3-spinel were fused with Al2O3 content of 70% and 90% respectively are produced in by electronical fusing furnaces. And it can be processed into the grains, the fine powders and the micro powders with different particle sizes.
Spinel property of index
Properties | AM-70 | AM-90 | |
Chemical Composition (%) | Al2O3 | 69-76 | 88-91 |
Grain Size (mm) | 3~5 | 3~5 | |
Fine powder(mesh) | 80,100,240,320,etc. | 80,100,240,320,etc. | |
Micro powder(μm) | 3~5 5~10 | 3~5 5~10 |